Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Fibre Intermediates Nyrim® 3000 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer DSM Fibre Intermediates
Trade Name Nyrim®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Fibre Intermediates Nyrim® 3000 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.Information provided by the manufacturer, Brueggemann Chemical.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.7 %
1.7 %
DIN 53714: 23°C, 50% Relative Humidity
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 868
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ISO 527
Elongation at Break 370 %
370 %
ISO 527
Modulus of Elasticity 0.431 GPa
62.5 ksi
ISO 527
Flexural Modulus 0.466 GPa
67.6 ksi
ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180, No break
30.0 kJ/m²

@Temperature -40.0 °C
14.3 ft-lb/in²

@Temperature -40.0 °F
Ductile break; ISO 180
Charpy Impact, Notched NB
NB
No break
NB
NB
Low Temp
Thermal Properties Metric English Comments
Melting Point 213 °C
415 °F
DSC
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+9 ohm-cm
4.00e+9 ohm-cm
DIN 53482
Surface Resistance 3.00e+8 ohm
3.00e+8 ohm
DIN 53482
Dielectric Constant 4.6

@Frequency 1e+6 Hz
4.6

@Frequency 1e+6 Hz
DIN 53483
14.9

@Frequency 50 Hz
14.9

@Frequency 50 Hz
DIN 53483
Dielectric Strength 13.0 kV/mm
330 kV/in
DIN 53481
Dissipation Factor 0.10

@Frequency 1e+6 Hz
0.10

@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 600 V
600 V
DIN IEC 112 / VDE 030 t1
Copyright © lookpolymers.com All Rights Reserved