Polymer Property : Volume Resistivity = 4.00e+9 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+9 ohm-cm
4.00e+9 ohm-cm
DIN 53482
DSM Fibre Intermediates Nyrim® 3000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..