Polymer Property : Surface Resistance = 3.00e+8 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 3.00e+8 ohm
3.00e+8 ohm
DIN 53482
DSM Fibre Intermediates Nyrim® 3000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Surface Resistance 3.00e+8 ohm
3.00e+8 ohm
ASTM D257
Arkema Group Pebax® MV1074 Polyether Block Amide
Surface Resistance 3.00e+8 ohm
3.00e+8 ohm
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista..