Daikin POLYFLON FA-500 MPA, White Powder

Category Polymer , Thermoplastic
Manufacturer Daikin Industries
Trade Name POLYFLON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Daikin POLYFLON FA-500 MPA, White Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White powder.Major Uses: Addition of a minute amount of resins produces excellent anti-dripping properties. Good dispersion into resins enables production of moldings with better appearance than with conventional PTFE.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Specific Gravity 2.18 g/cc
2.18 g/cc
Bulk Density 0.570 g/cc
0.0206 lb/in³
Particle Size 400 µm
400 µm
Average
Mechanical Properties Metric English Comments
Coefficient of Friction 0.020 - 0.038
0.020 - 0.038
0.020 - 0.0385
0.020 - 0.0385
Lubricating
Taber Abrasion, mg/1000 Cycles <= 98.1
<= 98.1
9.8 N load, cs-10 wheel
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
Electrical Properties Metric English Comments
Dielectric Constant 2.1

@Frequency 1000 Hz
2.1

@Frequency 1000 Hz
ASTM D150
2.1

@Frequency 1e+6 Hz
2.1

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.00010 - 0.00022
0.00010 - 0.00022
PTFE Component