LyondellBasell Astryn NXO-21001 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn NXO-21001 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: high melt flow, medium modulus polypropylene copolymer, high flow, excellent processability, excellent colorabilityApplications: wire harnesses, housings, thin walled partsDescription: Astryn NXO-21001 high melt flow, unreinforced polypropylene copolymer is designed for injection molding thin-walled parts. It combines good properties with excellent processability.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792B
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Tool, Montell
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Ultimate 19.0 MPa
2760 psi
ASTM D638
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 280 %
280 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648