Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS Cycoloy Medium Heat Plating Grade for Automotive |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East) Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® BFL4000U PC Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Europe-Africa-Middle East) Unreinforced PBT+PC alloy. Improved retention of mechanical properties under UV. Excellent low temperature/chemical |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ISO 180 |
Styrolution Styrolux® 3G46 SBC Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | |
Shandong Guangyin 1212 Reinforced Nylon Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cab.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -10.0 °C |
14.3 ft-lb/in² @Temperature 14.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ISO 180 |
Tisan TISLAMID® 66 Impact Modified Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -50.0 °C |
14.3 ft-lb/in² @Temperature -58.0 °F |
|
Dow LDPE 955I Low Density Polyethylene DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD4471 PC (Europe-Africa-Middle East) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |