California Fine Wire Alloy 422 Precious Metal Alloy

Category Metal , Nonferrous Metal , Precious Metal
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Alloy 422 Precious Metal Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 19.3 g/cc
0.698 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 1450 MPa
210000 psi
Stress relieved
1520 MPa
220000 psi
Hard
Modulus of Elasticity 221 GPa
32000 ksi
Thermal Properties Metric English Comments
Melting Point 1880 °C
3416 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000299 ohm-cm
0.0000299 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.0007 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.0024