Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D955
Melt Flow 11 g/10 min

@Load 8.70 kg,
Temperature 190 °C
11 g/10 min

@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.7 MPa
3580 psi
ASTM D412
Tensile Modulus 2.07 GPa
300 ksi
ASTM D412
Thermal Properties Metric English Comments
Vicat Softening Point 75.6 °C
168 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 193 - 210 °C
380 - 410 °F
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
Dry Time 2 - 4 hour

@Temperature 104 °C
2 - 4 hour

@Temperature 220 °F
to ensure moisture level is less than 0.02%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.000 - 0.345 MPa
0.000 - 50.0 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm