Processing Properties Metric English Comments
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy)
VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid)
60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible A5DUB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible A7501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible R8570A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 241 °C
380 - 465 °F
Processing
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 499 X 83696 Polystyrene (PS), Glass Fiber - Permanently Anti-static
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6003-75A Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6003-75A UV Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT - UV Stabilized
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6042-40A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6042-70A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 700 TFE 15 High Density Polyethylene (HDPE), PTFE Lubricated
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 727 High Density Polyethylene (HDPE), Talc
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 799 A X 99499 Low Density Polyethylene (LDPE), Glass Bubbles
Melt Temperature 193 - 216 °C
380 - 420 °F
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Melt Temperature 193 - 232 °C
380 - 450 °F
LTL Color Compounds ColorFast® FRA204 ABS
High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc.
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Total HL 428 HDPE Film Grade
Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro..
Melt Temperature 193 - 221 °C
380 - 430 °F
RTP Company PermaStat® 1500-50D Polyether-Ester Block Copolymer (TEEE/COPE), Permanently Anti-static - ESD Protection
Melt Temperature 193 - 216 °C
380 - 420 °F
RTP Company RTP 1200 S-80A Ester-based Thermoplastic Polyurethane Elastomer
Melt Temperature 193 - 210 °C
379 - 410 °F
Molding
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Melt Temperature 193 - 210 °C
379 - 410 °F
Molding
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Melt Temperature 193 °C
380 °F
Axiall 19481 Wire & Cable Flexible PVC
105°C, VW-1 rated non-lead stabilized insulation. Best suited for small gauge, 1/64 wall applications. UL approved for TW, THW, THHW, THHN-THWN insulation.Information provided by Georgia GulfGeor..
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
Melt Temperature 193 - 210 °C
380 - 410 °F
Extrusion
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set ..
Melt Temperature 193 - 227 °C
380 - 440 °F
RTP Company RTP 2800 B-75A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Melt Temperature 193 - 227 °C
380 - 440 °F
RTP Company RTP 2800 B-65A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Melt Temperature 193 - 232 °C
379 - 450 °F
Injection
Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerBK13 is an SBC developed specifically to have enhanced flow capabilities and improved stiffness over the KR01 grade. BK13 molded parts give excellent detail on rapid prod..
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6042-60A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested