Processing Properties Metric English Comments
Melt Temperature 193 - 216 °C
380 - 420 °F
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6003-45A Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6003-55A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6042-60A Specialty Thermoplastic Elastomer, PC/ABS Bondable
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6042-60A Z Specialty Thermoplastic Elastomer
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 700 A FR Low Density Polyethylene (LDPE), Flame Retardant
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 700 TFE 15 High Density Polyethylene (HDPE), PTFE Lubricated
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 799 A X 99499 Low Density Polyethylene (LDPE), Glass Bubbles
Melt Temperature 193 °C
380 °F
Spartech E66091 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Melt Temperature 193 °C
380 °F
Processing Temperature
Teknor Apex APEX® 1020 Polyvinyl Chloride, Semi-Rigid
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer
A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje..
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
Melt Temperature 193 - 221 °C
380 - 430 °F
RTP Company EMI 161 Polypropylene (PP), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 2740 S-40A Z Saturated Styrenic Block Copolymer, FDA Compliant Ingredients
Melt Temperature 193 - 216 °C
380 - 420 °F
RTP Company RTP 1207 S-65D Ester-based Thermoplastic Polyurethane Elastomer, Glass Fiber
Melt Temperature 193 - 210 °C
380 - 410 °F
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester
Data provided by Clariant Masterbatches
Melt Temperature 193 °C
380 °F
Axiall 21540 Coax & Telecom Flexible PVC
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation.Information provided by Georgia GulfGeorgi..
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3140 can be processed by injection molding or extrusion for appl..
Melt Temperature 193 - 241 °C
380 - 465 °F
Processing
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Melt Temperature 193 - 216 °C
380 - 420 °F
Molding
PolyOne Lubri-Tech™ AT-10GF-10KV/000 Acetal-Copolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedAramid Fiber ReinforcedInformation provided by PolyOne Corporation.
Melt Temperature 193 - 210 °C
380 - 410 °F
Molding
PolyOne Edgetek® AT-30GB/000 Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation.
Melt Temperature 193 - 227 °C
380 - 440 °F
RTP Company RTP 2800 B-55A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Melt Temperature 193 - 227 °C
380 - 440 °F
RTP Company RTP 2800 B-65A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Melt Temperature 193 - 227 °C
380 - 440 °F
RTP Company RTP 2800 D-45A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex..
Melt Temperature 193 - 232 °C
380 - 450 °F
Processing
ExxonMobil Santoprene® 241-45 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water. This grade ..
Melt Temperature 193 - 241 °C
380 - 465 °F
Processing
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Melt Temperature 193 - 216 °C
380 - 420 °F
Molding
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 193 - 232 °C
380 - 450 °F
Average value: 213 °C Grade Count:3