Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips HiD® 9354 HDPE Natural Pipe Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips HiD® 9354 HDPE Natural Pipe Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: gas phase linear hexane copolymerApplications: corrugated pipe applicationsInformation provided by Chevron Phillips Chemical Company.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 24 hour
>= 24 hour
Condition B; ASTM D 1693
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Ultimate 28.3 MPa
4100 psi
ASTM D638
Tensile Strength, Yield 16.5 MPa
2390 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
2% Secant; ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Users viewing this material also viewed the following: