Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Faradex NSL121 PC+ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Antistat/Conductive , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Faradex NSL121 PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* NSL121 is a compound based on PC+ABS Blend resin containing Stainless Steel Fiber, PTFE, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Internally Lubricated, Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
5 mm/min; ISO 527
Elongation at Yield 4.1 %
4.1 %
5 mm/min; ISO 527
Tensile Modulus 2.90 GPa
421 ksi
1 mm/min; ISO 527
Flexural Yield Strength 92.0 MPa
13300 psi
2 mm/min; ISO 178
Flexural Modulus 2.90 GPa
421 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 57.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
31.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D 257
Users viewing this material also viewed the following: