Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
Chevron Phillips HiD® 9352 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: corrugated pipe applicationsInformation provided by Chevron .. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
Chevron Phillips HiD® 9354 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymerApplications: corrugated pipe applicationsInformation provided by Chevron Phillips Chemical Company. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM Data |
Styron Magnum™ HPC 952 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
American Polymers API 410 Polystyrene API 410 is a low impact polystyrene with very high gloss and superior dimensional stability.Applications: API 410 is ideally suited for point of purchase displays where high gloss and some impact i.. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
DuPont™ Surlyn® 9150 Ionomer Resin, Zinc Surlyn® 9150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The high MAA content and mi.. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
Buckeye Polymers BP RPP 2020T Polypropylene, 20% Mineral Filled This Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resis.. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
Buckeye Polymers BP RPP 2508 T Polypropylene, 25% Mineral Filled This Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resis.. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
Adell RA-14 Copolymer Polypropylene, 20% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 28.3 MPa | 4100 psi | ASTM D638 |
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |