Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® BS-70 70% Barium Sulfate Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® BS-70 70% Barium Sulfate Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® BS series compounds are homopolymer polypropylene resins reinforced with barium sulfate. They possess increased specific gravity, high flex modulus, high deflection temperature, good chemical resistance, frictional resistance, and x-ray opacity.Applications: Cosmetic applicationMolded weightsSoundproofing componentsMedical devicesStandard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ASTM D792
Filler Content 70 %
70 %
ASTM D2584
Melt Flow 6.0 - 14 g/10 min
6.0 - 14 g/10 min
May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.3 MPa
2800 psi
ASTM D638
Flexural Modulus 3.81 GPa
552 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.149 J/cm
0.280 ft-lb/in
At 73°F; ASTM D256
Izod Impact, Unnotched 1.48 J/cm
2.78 ft-lb/in
At 73°F; ASTM D256
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved