Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-2753 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | Exxon Method |
ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2717 HDPE Injection Molding Resin
(discontinued **) Features: Super high flow, good balance of toughness and stiffness, low odor, permits container weight reduction.Applications: Thin walled food containers.Data provided by the manufacturer. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1183 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® LH5326 Injection Molding HDPE
(discontinued **) CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5326 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HP5221 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP5221 is a high performance copolymer that is designed for the most demanding requirements of corrugated pipe applications. Formolene® HP5221 meets the re.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5332CP High Density Polyethylene ApplicationsALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resis.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® M5363 High Density Polyethylene ApplicationsALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properti.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5004 1000 Micron EVA Powder Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a viny.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos B4020N1332 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos CP53-30 Polyethylene Copolymer CP53-30 is a high density polyethylene copolymer developed for corrugated piping applications. This product is recommended for use in applications that are required to meet AASHTO specifications M 2.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos T50-500 HDPE Ineos T50-500 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and en.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos T50-500-171 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos T50-800-01 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Density | 0.953 - 0.959 g/cc | 0.0344 - 0.0346 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 4950 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.953 - 0.961 g/cc | 0.0344 - 0.0347 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 5240 PR HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5226 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5301 EA HDPE Blow Molding Applications:High performance blow molded containers typically of to 60 liters capacity for packaging aggressive productsRobust industrial and technical moldingsInformation provided by Interchim s.r.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1183 |
Borealis BorSafe™ HE3495-LS HDPE Compound BorSafe™ HE3495-LS is a bimodal polyethylene compound produced by the advanced Borstar® technology. It's fully stabilized against thermal degradation and the die build-up during extrusion is minim.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1183 |
Borealis Borstar® HE3498-LS Orange-Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Natural Gas Borstar HE3497-LS is a bimodal, cadmium free, high density polyethylene compound designed for coextrusion of blue identifying stripes. It is fully stabilized against thermal degradation and the die.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® AD2528 Adhesive Application Resin Escorene Ultra AD 2528 is a very high flow rate, 27.6% Vinyl Acetate, copolymer, which is useful in formulating hot melt adhesives.Availability: Latin America, North America and South America Additi.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ AA53-003 Pipe Extrusion Resin Product Description: AA53-003 is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | |
Dow HDPE 65053N High Density Polyethylene DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellen.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® B592 Polyethylene, Injection Molding Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil Paxon™ BA53-035 Blow Molding Resin
(discontinued **) BA53-035 is a high molecular weight, high density polyethylene copolymer offering an outstanding combination of stiffness and toughness. The resin provides superior melt strength and impact resista.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | Exxon Method |
ExxonMobil Iotek® 7310 Zinc Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer.Applications: Injection molding; Impact modifier of polyamide. |