Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass and Mineral Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 945 is an ESD level Conductive grade of Bulk Molding Compound and is suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is well suited for injection molding.Typical applications may include electronic enclosures, computer chip trays and storage boxes, and other applications requiring ESD level conductivity.
Physical Properties Metric English Comments
Specific Gravity 1.75 - 1.95 g/cc
1.75 - 1.95 g/cc
Water Absorption 0.14 - 0.21 %
0.14 - 0.21 %
24 hours, 23°C
Linear Mold Shrinkage 0.0050 - 0.010 cm/cm
0.0050 - 0.010 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 55
45 - 55
Tensile Strength, Ultimate 41.4 - 51.7 MPa
6000 - 7500 psi
Flexural Strength 82.7 - 96.5 MPa
12000 - 14000 psi
Flexural Modulus 12.4 - 13.8 GPa
1800 - 2000 ksi
Compressive Strength 124 - 138 MPa
18000 - 20000 psi
Izod Impact, Notched 1.07 - 1.60 J/cm
2.00 - 3.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 232 °C
>= 450 °F
Glass Transition Temp, Tg >= 165 °C
>= 329 °F
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Electrical Properties Metric English Comments
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F