Material Notes:
Nontoxic alternative to traditional materials, radiation shielding applications.Moderate Specific GravityBaSO4 Powder Filled ABSInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Internal
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
ISO 527
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ISO 527
Flexural Modulus 8.00 GPa
1160 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Thickness 3.20 mm
2.86 ft-lb/in²

@Thickness 0.126 in
ISO 180-A
Processing Properties Metric English Comments
Melt Temperature 250 - 265 °C
482 - 509 °F
Mold Temperature 55.0 - 80.0 °C
131 - 176 °F
Drying Temperature 90.0 °C
194 °F
Dry Time 2 - 4 hour
2 - 4 hour