Borealis Daplen™ EE260AI Polypropylene TPO Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Mica Filler , Polypropylene, Mineral Reinforced
Manufacturer Borealis
Trade Name Daplen™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Daplen™ EE260AI Polypropylene TPO Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Daplen™ EE260AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. Applications: Daplen™ EE260AI has been developed especially for the car industry to be used in automotive interior parts including pillar trims, door panels and pockets, dashboards, and automotive interior applications.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
mold average;Borealis Method
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
56 g/10 min

@Load 5.00 kg,
Temperature 230 °C
56 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
50mm/min; ISO 527-2
Elongation at Yield 6.0 %
6.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.80 GPa
261 ksi
1mm/min; ISO 527-2
Flexural Strength 28.0 MPa
4060 psi
ISO 178
Flexural Modulus 1.90 GPa
276 ksi
2mm/min; ISO 178
Charpy Impact Unnotched 7.00 J/cm²

@Temperature -20.0 °C
33.3 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ISO 75-2
Vicat Softening Point 52.0 °C

@Load 5.10 kg
126 °F

@Load 11.2 lb
ISO 306
130 °C

@Load 1.02 kg
266 °F

@Load 2.25 lb
ISO 306
Processing Properties Metric English Comments
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Feed Temperature 40.0 - 80.0 °C
104 - 176 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Velocity 100 - 200 mm/sec
3.94 - 7.87 in/sec
Hold Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Descriptive Properties Value Comments
Back Pressure low to medium
Emission (µgC/g) < 50
VDA 277
Fogging (mg) < 2
DIN 75201;100°C, 16h
Screw Speed low to medium