Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Lord Adhesives
Trade Name Chemglaze®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. These films provide excellent tensile and elongation properties, and prevent corrosion of metal substrates in aggressive environments.Basic UsesChemglaze elastomeric polyurethane coatings function especially well in abrasive environments. With their inherent flexibility, corrosion resistance and energy absorptive properties, these coatings are used in the railroad and mining industries to protect metallic substrates. Chemglaze elastomeric coatings accommodate thermal expansion and contraction as well as structural motion. These elastic properties make them useful in protecting spray applied polyurethane foam insulation on storage tanks and reactor vessel walls.These coating qualify under military rain erosion coating specification MIL-C-85322.All information provided by Lord.
Physical Properties Metric English Comments
Solids Content 7.5 %
7.5 %
M201; by volume
9.0 %
9.0 %
M201; by weight
52 %
52 %
Mixed; by volume
56 %
56 %
Mixed; by weight
67 %
67 %
M331; by volume
73 %
73 %
M331; by weight
Volatile Organic Compounds (VOC) Content 420 g/l
420 g/l
Brookfield Viscosity 0.89 cP

@Temperature 25.0 °C
0.89 cP

@Temperature 77.0 °F
Part B, M201; LVT, Spindle #4 @ 30rpm
8500 cP

@Temperature 25.0 °C
8500 cP

@Temperature 77.0 °F
Part A, M331; LVT, Spindle #4 @ 30rpm
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D882-83, Method A
Elongation at Yield 500 %
500 %
ASTM D882-83, Method A
Taber Abrasion, mg/1000 Cycles 0.00
0.00
CS17 1000g/1000cycles; ASTM D4060
60
60
H18 1000g/1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Flash Point 33.9 °C
93.0 °F
Part A, M331; Setaflash
43.3 °C
110 °F
Part B, M201; Setaflash
Processing Properties Metric English Comments
Cure Time 15.0 - 30.0 min
0.250 - 0.500 hour
Set to Touch
60.0 - 120 min
1.00 - 2.00 hour
Surface Dry
240 - 360 min
4.00 - 6.00 hour
Dry Hard
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
50% relative humidity
Shelf Life 6.00 Month

@Temperature 24.0 °C
6.00 Month

@Temperature 75.2 °F
Part A, M331
6.00 Month

@Temperature 24.0 °C
6.00 Month

@Temperature 75.2 °F
Part B, M201
Descriptive Properties Value Comments
Appearance Black
Part A, M331
Black
Mixed
Yellow to Dark Amber
Part B, M201
Weight per Gallon (lbs) 7
Part B, M201
8.4
Part A, M331
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved