Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 56 g/10 min @Load 5.00 kg, Temperature 360 °C |
56 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re.. |
|||
Melt Flow | 56 g/10 min @Load 5.00 kg, Temperature 360 °C |
56 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Melt Flow | 56 g/10 min @Load 5.00 kg, Temperature 360 °C |
56 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Melt Flow | 56 g/10 min @Load 5.00 kg, Temperature 360 °C |
56 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for.. |
|||
Melt Flow | 56 g/10 min @Load 5.00 kg, Temperature 360 °C |
56 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem EXUM0169 PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Melt Flow | 56 g/10 min @Load 5.00 kg, Temperature 230 °C |
56 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EE260AI Polypropylene TPO Compound Daplen™ EE260AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |