Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Die Temperature | 210 - 241 °C | 410 - 466 °F | |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Die Temperature | 210 °C | 410 °F | |
Taiwan PU Corporation TPU-E95 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
Die Temperature | 210 - 230 °C | 410 - 446 °F | |
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Die Temperature | 210 °C | 410 °F | Body |
SK Chemicals SKYTHANE® R155D Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BA204E Polypropylene Block Copolymer for Non-Pressure Pipes BA204E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA204E is recommended for non-pressure pipes & fittings, thin-walle.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating Borcoat™ MA115E is a highly filled polypropylene compound and is self colored. Applications: Borcoat™ MA115E is recommended as heavy weight coating for special applications used in steel pipe coa.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6015 Polypropylene Random Copolymer RA130E-6015 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Die Temperature | 210 °C | 410 °F | Zone 2, Extrusion |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection.. |
|||
Die Temperature | 210 °C | 410 °F | 6, Zone 1, Extrusion |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Die Temperature | 210 °C | 410 °F | 6, Zone 1, Extrusion |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |
|||
Die Temperature | 210 °C | 410 °F | Zone 2, Extrusion |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6020 Polypropylene Random Copolymer RA130E-6020 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Die Temperature | 210 - 240 °C | 410 - 464 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1502E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 210 - 240 °C | 410 - 464 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1655E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Appeel® 72D811 Sealing Resin DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion.. |
|||
Die Temperature | 210 °C | 410 °F | Blown Film Coextrusion |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Die Temperature | 210 °C | 410 °F | Extrusion Coating |
DuPont™ Elvaloy® AC34035 Ethylene Methyl Acrylate Elvaloy® AC 34035 is a copolymer of ethylene and butyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A.. |
|||
Die Temperature | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® E185SB Ionomer Resin Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed.. |
|||
Die Temperature | 210 °C | 410 °F | Extrusion |
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Die Temperature | 210 °C @Pressure 4.80 - 17.0 MPa |
410 °F @Pressure 696 - 2470 psi |
Extrusion |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Pipe Extrusion |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Die Temperature | 210 - 260 °C | 410 - 500 °F | Average value: 247 °C Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |