Material Notes:
Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under load is excellent. It maintains its inherent chemical resistance to greases, oils and hydrocarbons. It is available in natural and black versions. Pigmented and weatherable versions may be offered on a case by case basis.Applications: consumer power tool housings, cattle ear taggers, luggage frames, fans and pressure regulator housings.Information provided by BASF
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.90 %
0.90 %
24 hour; ISO 62
1.5 %
1.5 %
50% RH; ISO 62
5.2 %
5.2 %
Saturation; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Flexural Strength 290 MPa
42100 psi
ISO 178
Flexural Modulus 1.18 GPa
171 ksi
ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ISO 3146
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
UL RTI, Electrical 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
746B
UL RTI, Mechanical with Impact 105 °C

@Thickness 1.50 mm
221 °F

@Thickness 0.0591 in
746B
UL RTI, Mechanical without Impact 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
746B
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 280 - 305 °C
536 - 581 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.060 %
<= 0.060 %
Descriptive Properties Value Comments
Color BK 102
Commercial Status North America