Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 7699 BLK Multi-Flex® A 7699 is an acoustic barrier compound for medium density applications . Multi-Flex® TPE compounds are based on Shell Kraton G polymers licensed to Multibase. Multi-Flex TPE contains.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8699 BLK Multi-Flex® A 8699 is a TPE compound based on Kraton G polymer. It is used as medium density acoustic for noise abatement in the auto industry. Multi-Flex TPE contains Kraton™ G.Data provided by.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | STN 64 0111 |
Plastcom SLOVAMID 6 GF 25 FRA 5 Polyamide 6, 25% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
PolyOne Nymax™ GMF 604 40 UV Black 148 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | STN 64 0111 |
Plastcom SLOVAMID 66 GF 30 FRA 5 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792, ISO 1183 |
Nilit Nilitop BT G2 FR C3 is a 10% Glass Fiber Reinforced, Flame Retardant PBT Description: Nilitop BT G2 FR C3 is a 10% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hylon® N2040MHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 410 Rigid PVC, Extrusion Clic channels |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, DRY Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183/A |
Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6 Description: TECHNYL B 52 G1 MX35 is a copolyamide 6.6/6 , with thermal protection, glow wire resistant and reinforced with mineral filler.Colors: GreyAvailable in: Latin AmericaMain Properties: ? G.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66 LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM AR9300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF30 TL5 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Low Extracta.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF43 ML2 BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 43% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated Appearance: BlackTPCI# 8047101Informa.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GF006 is a compound based on Polysulfone resin containing Glass Fiber. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183-87 |
Wellman Wellamid® MRGF25/15 42H-BKDX9 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183-87 |
Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced Improved surface appearance gradeAll information provided by Wellman Engineered Resins. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-111 Compression Molded PEEK Compound, 50% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 82 Flexible PVC, Sheathing General purposes |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds FKA 0753 Flexible PVC, Flame Retardant Insulation Lead Free General purposes |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR23 BK EF PBT, 23% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade Information provided by Eurotec® |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 408 BK515 PET Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | |
BASF Paliogen® Red Violet L 5100 Color Additive Description: Quinacridone pigment especially for bordeaux and maroon shade Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by .. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | Sintered; ASTM D792 |
ALM PA-615-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |
|||
Density | 1.49 - 1.82 g/cc | 0.0538 - 0.0658 lb/in³ | Average value: 1.63 g/cc Grade Count:38 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |