BASF Novolen® 1040 N Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Novolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Novolen® 1040 N Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nucleated grade for injection molded parts.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
Water Absorption 0.10 %
0.10 %
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
Elongation at Break 20 %
20 %
Elongation at Yield 7.0 %
7.0 %
Tensile Modulus 2.00 GPa
290 ksi
Charpy Impact Unnotched 11.0 J/cm²
52.4 ft-lb/in²
1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
0.150 J/cm²

@Temperature -30.0 °C
0.714 ft-lb/in²

@Temperature -22.0 °F
Tensile Creep Modulus, 1 hour 700 MPa
102000 psi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
Melting Point 165 °C
329 °F
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Vicat Softening Point 102 °C
216 °F
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.3

@Frequency 100 Hz
2.3

@Frequency 100 Hz
2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
Dielectric Strength 140 kV/mm
3560 kV/in
Dissipation Factor 0.000070

@Frequency 100 Hz
0.000070

@Frequency 100 Hz
0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
600 V