Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792-91 |
Multibase Multi-Flex® TPO D-5016 Multi-Flex® D-5016 is an elastomer modified polypropylene for applications requiring elastomeric properties and good molding behavior.Data provided by Multibase. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
Plastcom SLOVALEN PQ 83 N PP, imp. strength FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D4883 |
Westlake Mxsten CV CV77515-F Plastomer
(discontinued **) Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 10B Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, excellent dart impact, excellent clarity.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D1475 |
Humiseal 1B31 Acrylic Conformal Coating Humiseal 1B31 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C ApprovedPasses thermal shock test (MI.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
LyondellBasell Plexar® PX3216 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | Not Compounded |
KKPC KOSYN KBR 01 Polybutadiene Rubber (High cis BR) Polybutadiene Rubber (High cis BR)Characteristics: Polybutadiene Rubber (BR), which has three kinds of bond structure of cis-1,4, trans-1,4, vinyl, is simple polymer made from 1,3-butadiene by solut.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
Global PPC-0320 Standard Grade Polypropylene Information provided by Global Polymers Corporation. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
Mitsui ADMER® NF488A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 5703 BLK The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
Mitsui ADMER® NF498A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
LyondellBasell Hostacomâ„¢ TRC704D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TRC704D medium high melt flow, 1,500 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and proce.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
Styron Buna® cis 132 Schkopau High-cis Polybutadiene Rubber (PBR) Composition: Buna® cis 132 – Schkopau is a stereospecific polybutadiene with a high 1,4-cis content. It is manufactured by a solution process using an organo-metallic nickel catalyst which p.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Borealis BG373MO Polypropylene Copolymer BG373MO is a heterophasic copolymer. Products molded with this grade exhibit excellent antistatic performance and very good mould release. Electrostatic charge is |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Borealis BH374MO Polypropylene Copolymer BH374MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. Products molded with this grade exhibi.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
UBE UBEPOL VCR303 Synthetic Rubber (Raw Polymer) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D1505 |
UBE UBEPOL VCR406 Synthetic Rubber (Raw Polymer) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
Diamond Polymers NPP30-2000HC Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP) AFFINITY™ PT 1409 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies from Dow Plastics. Resin blended with 20 wt% LDPE to improve extrusion coating performance.Information provided b.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow Engage® 8445 Polyolefin Elastomer Description: Engage® 8445 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |
|||
Density | 0.911 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow FLEXOMER™ ETS-9064 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Density | 0.910 - 0.950 g/cc | 0.0329 - 0.0343 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ CAT 103T Catalyst for Cable Compound Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• High reactive cataylstInformation provided by Fainplast Compounds |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ISO 1183 |
Arkema Group OREVAC® 18751 Maleic Anhydride Modified Polypropylene DescriptionOREVAC 18751 is a coextrusion coating adhesive based on a maleic anhydride modified polypropylene resin. It combines the processability of an extrusion coating resin with the thermal resi.. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
BASF Novolen® 2500 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | ASTM D792 |
Buckeye Polymers BP Flex D8020 UC85 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D1505 |
PolyOne Syncure™ S1042A Polyethylene, Crosslinked (XLPE) Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Deformation, and Gel measured on a 95 phr S1042A / 5 phr S1000B system; and cured .. |
|||
Density | 0.910 g/cc | 0.0329 lb/in³ | |
BASF Novolen® 1102 L Polypropylene Data was collected by ISO methods and provided by BASF. |