BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and performance under load. It maintains excellent chemical resistance to greases, oils and hydrocarbons. It is available in natural and black.Capron 8230G HS is generally recommended for applications such as gears and consumer weed trimmer parts. ASTM Callout PA220 G06 A29140 UB032.Data provided by Allied Signal.Processing: Max. water content 0.16%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.Melt Temperature: 250-280 degC (482-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate. Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO data
Water Absorption 1.5 %
1.5 %
24 hrs; ISO data
Moisture Absorption at Equilibrium 2.5 %
2.5 %
50% RH; 23°C; ISO data
Water Absorption at Saturation 8.9 %
8.9 %
in water; 23°C; ISO data
Viscosity Measurement 50
50
Formic Acid Viscosity; ISO data
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM Data MD
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
Same value from ASTM and ISO tests; 5 mm/min.
Elongation at Break 4.3 %
4.3 %
ISO, 5 mm/minl
5.0 %
5.0 %
ASTM, 5 mm/minl
Flexural Yield Strength 125 MPa
18100 psi
ASTM Data
Flexural Modulus 3.44 GPa
499 ksi
ISO Value
3.86 GPa
560 ksi
ASTM Value
Poissons Ratio 0.35
0.35
ISO data
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO Data
Thermal Properties Metric English Comments
CTE, linear 59.0 µm/m-°C

@Temperature 20.0 °C
32.8 µin/in-°F

@Temperature 68.0 °F
ASTM data
Melting Point 220 °C
428 °F
ASTM and ISO test
Deflection Temperature at 1.8 MPa (264 psi) 192 °C
378 °F
ASTM Data
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Processing Properties Metric English Comments
Processing Temperature 275 °C
527 °F
See Materials Notes
Mold Temperature 95.0 °C
203 °F
See Materials Notes
Drying Temperature 85.0 °C
185 °F
See Materials Notes