Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 59.0 - 108 µm/m-°C | 32.8 - 60.0 µin/in-°F | Average value: 94.6 µm/m-°C Grade Count:9 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini.. |
|||
CTE, linear | 59.0 µm/m-°C @Temperature 20.0 °C |
32.8 µin/in-°F @Temperature 68.0 °F |
ASTM D228 |
Dow INSPIRE™ D7000 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
CTE, linear | 59.0 µm/m-°C @Temperature 20.0 °C |
32.8 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Polycasa COPOL PETG QUINN COPOL has good optical properties, brilliant surface, easy to vacuum form without pre-drying, low water absorption, very good chemical resistance, and high impact properties.Bus shelters (UV-v.. |
|||
CTE, linear | 59.0 µm/m-°C @Temperature 20.0 °C |
32.8 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor.. |
|||
CTE, linear | 59.0 µm/m-°C @Temperature 40.0 - 130 °C |
32.8 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 2000 Phenolic, Granular, Compression Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
CTE, linear | 59.0 µm/m-°C @Temperature 40.0 - 130 °C |
32.8 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 2308 Phenolic, Granular, Injection Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
CTE, linear | 59.0 µm/m-°C | 32.8 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de.. |
|||
CTE, linear | 59.0 µm/m-°C | 32.8 µin/in-°F | Below Tg |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
CTE, linear | 59.0 µm/m-°C @Temperature 20.0 °C |
32.8 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 807 High Performance Epoxide 10 Minute Set, Non-Sagging, 1:1, Excellent Electrical & Mechanical Properties |
|||
CTE, linear | 59.0 µm/m-°C | 32.8 µin/in-°F | ASTM E831-93 |
Saint-Gobain Meldin® 2030 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |