Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Multibase Multi-Pro® 4005 M Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the .. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standa.. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
PolyOne Edgetek® CY-10GF/000 UV FR V0 NATURAL PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedNon-HalogenatedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Covestro Petlon® PC/PET 36A 620UV Yellow Semi-Crystalline PET, 10% Glass Fiber
(discontinued **) Characteristics: Good Thermal and Dimensional Stability, Good Chemical ResistanceApplications: Automotive Panels, Electronic Housings, Pump HousingsProcessing: Injection Molding (Melt Temperature: 5.. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM Value |
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor.. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM Data |
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l.. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM Data |
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista.. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK) KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr.. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp PH0700B PA 6 LNP* Thermocomp* PH0700B is a Nylon 6 base resin containing Tungsten. Characteristics are High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 (Asia Pacific) LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFRMPPCC-30 30% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFPC 5010 Glass Filled Polycarbonate AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Asahi Kasei Thermylene® F6-30FG-0100 30% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.86 GPa | 560 ksi | ASTM D790 |
Asahi Kasei Thermylene® P-25FG-0100 25% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.86 - 17.5 GPa | 560 - 2540 ksi | Average value: 10.1 GPa Grade Count:44 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |