Polymer Property : Flexural Modulus = 3.86 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Multibase Multi-Pro® 4005 M Polypropylene
Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the ..
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standa..
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
PolyOne Edgetek® CY-10GF/000 UV FR V0 NATURAL PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedNon-HalogenatedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Covestro Petlon® PC/PET 36A 620UV Yellow Semi-Crystalline PET, 10% Glass Fiber  (discontinued **)
Characteristics: Good Thermal and Dimensional Stability, Good Chemical ResistanceApplications: Automotive Panels, Electronic Housings, Pump HousingsProcessing: Injection Molding (Melt Temperature: 5..
Flexural Modulus 3.86 GPa
560 ksi
ASTM Value
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor..
Flexural Modulus 3.86 GPa
560 ksi
ASTM Data
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l..
Flexural Modulus 3.86 GPa
560 ksi
ASTM Data
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista..
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)
KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced..
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr..
Flexural Modulus 3.86 GPa
560 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp PH0700B PA 6
LNP* Thermocomp* PH0700B is a Nylon 6 base resin containing Tungsten. Characteristics are High Specific Gravity.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 3.86 GPa
560 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6
LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 3.86 GPa
560 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 (Asia Pacific)
LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 3.86 GPa
560 ksi
Tangent; ASTM D790
Plastics Group Polifil® GFRMPPCC-30 30% Glass Reinforced Polypropylene, High Impact
Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap..
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Aaron Industries AAROPRENE® GFPC 5010 Glass Filled Polycarbonate
AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Asahi Kasei Thermylene® F6-30FG-0100 30% Glass Fiber Reinforced, Chemically Coupled
Information provided by Asahi Thermofil
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Asahi Kasei Thermylene® P-25FG-0100 25% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.86 - 17.5 GPa
560 - 2540 ksi
Average value: 10.1 GPa Grade Count:44
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..