Axiall 3027 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 3027 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 3027 is a powder blend designed as a substrate base for coextruded profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
ASTM D-2240
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Tensile Modulus 2.72 GPa
395 ksi
ASTM D-638
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D-790
Izod Impact, Notched 1.87 J/cm

@Temperature 23.0 °C
3.50 ft-lb/in

@Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
ASTM D-648
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F