Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 41.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Omni Plastics OmniTuff™ HPP GRC10 Homopolymer Polypropylene Glass Reinforced
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Tensile Strength, Yield 41.4 MPa
6000 psi
51 mm/min; ASTM D638
PolyOne Edgetek® XT X XT 1001 Natural Copolyester
Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget..
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 41.4 MPa
6000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® AT-20GB/000 Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 41.4 MPa
6000 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® FRA204 ABS
High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES Elastoblend® PA6 IM 811 HS L (Conditioned)
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedTPCI# 6109102Information provided by TP Comp..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES Electrablend® POM C BK Acetal
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive and CopolymerAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech Korad® SP-9011 Cap ABS Sheet
Description: ABS SheetInformation provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet
Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Spartech SP-9013 FR/ABS Flame Retardant Sheet
Description: Flame Retardant SheetInformation provided by Spartech.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM Data
Styron Magnumâ„¢ 2642 ABS, Impact Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 41.4 MPa

@Thickness 3.20 mm
6000 psi

@Thickness 0.126 in
Injection Molded; ASTM D638
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM Data
Styron Magnumâ„¢ 342EZ ABS, Medium Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Techmer ES Luriblend® POM CO TL20 LE Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction, Low Extractables and CopolymerUL File Number: E..
Tensile Strength, Yield 41.4 MPa
6000 psi
Longitudinal
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.003" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Tensile Strength, Yield 41.4 MPa
6000 psi
Longitudinal
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.005" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Tensile Strength, Yield 41.4 MPa
6000 psi
Longitudinal
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.010" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Formosa Plastics Formolon® AWS Compound
AWS Powder Profiler Compound Series The AWS compounds have been designed for profile extrusion in indoor and non-weatherable applications and substrates for outdoor applications. They exhibit a natu..
Tensile Strength, Yield 41.4 - 89.6 MPa
6000 - 13000 psi
0.2% offset
Eagle Brass 101 OFE COPPER (Certified), Annealed
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall MP-6585 Rigid PVC, Molding
Georgia Gulf MP-6585 is an electrical grade rigid vinyl injection molding compound processing good strength, stiffness, toughness, and flow. In addition, it has excellent processing stability and s..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall SP-7107 Rigid PVC, Molding
Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall 7055 Rigid PVC, Extrusion
Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat..
Tensile Strength, Yield 41.4 - 127 MPa
6000 - 18400 psi
Average value: 62.7 MPa Grade Count:37
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Oxford Polymers H-Acetal 20PTFE 20% PTFE Reinforced Homopolymer Acetal  (discontinued **)
20% PTFE Reinforced Homopolymer AcetalInformation provided by Oxford Polymers.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Axiall 3027 Rigid PVC, Extrusion
Georgia Gulf 3027 is a powder blend designed as a substrate base for coextruded profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM 638
PlastxWorld CEVIAN® SER20 ABS
General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat..
Copyright © lookpolymers.com All Rights Reserved