Mechanical Properties Metric English Comments
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
Type S; ASTM D1822
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics.
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
ASTM D1822
ExxonMobil Paxon™ AA60-003 Blow Molding Resin
Product Description: AA60-003 is a medium molecular weight distribution high density polyethylene which is characterized by high stiffness, excellent melt uniformity, and chemical inertness.Availabi..
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
Compression molded; ASTM D1822, Type S
Dow 620I Linear Low Density Polyethylene (LDPE)
For extruded foam applications Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
ASTM D-1822
Axiall 7020 Rigid PVC, Extrusion
Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF..
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
ASTM D-1822
Axiall 3027 Rigid PVC, Extrusion
Georgia Gulf 3027 is a powder blend designed as a substrate base for coextruded profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.