Tensile Modulus 2.72 GPa
395 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2160 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.72 GPa
395 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.72 GPa
395 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycolac® MG37EPX ABS
ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L)
Tensile Modulus 2.72 GPa
395 ksi
ASTM D638
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Modulus 2.72 GPa
395 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy)
Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne
Tensile Modulus 2.72 GPa
395 ksi
ISO 527-1/-2
Kuraray Genestarâ„¢ N1000A-M41 Nylon
Standard unreinforced injection grade. Main features:Low water absorptionChemical ResistanceExamples of application are:Friction and wear applicationGear and Wheel
Tensile Modulus 2.72 GPa
395 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66
LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant.
Tensile Modulus 2.72 GPa
395 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT
LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Tensile Modulus 2.72 GPa
395 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Tensile Modulus 2.72 GPa
395 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL NH5020 PPE+PS
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Tensile Modulus 2.72 GPa
395 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Tensile Modulus 2.72 GPa
395 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Tensile Modulus 2.72 GPa
395 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS
EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l..
Tensile Modulus 2.72 GPa
395 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific)
Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad..
Tensile Modulus 2.72 GPa
395 ksi
ASTM D-638
Axiall 3121 Rigid PVC, Extrusion
Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is sui..
Tensile Modulus 2.72 GPa
395 ksi
ASTM D-638
Axiall 3217 Rigid PVC, Extrusion
Georgia Gulf 3217 is a powder blend designed for the extrusion of window, door, fence and marine profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia..
Tensile Modulus 2.72 GPa
395 ksi
ASTM D-638
Axiall 8264 Rigid PVC, Extrusion
Georgia Gulf 8264 is a rigid PVC pellet compound suited for applications where transparency is important. 8264 is widely used for clear films, sheets, and profile shapes in the packaging industry. ..
Tensile Modulus 2.72 GPa
395 ksi
ASTM D-638
Axiall 3027 Rigid PVC, Extrusion
Georgia Gulf 3027 is a powder blend designed as a substrate base for coextruded profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.