Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Atom Adhesives AA-BOND 2110 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-BOND 2110 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, nonsag, non-drip and improved impact strength properties are required. AA-BOND 2110 is easy-to-use two parts adhesive system contains no volatile solvents, readily cures at room temperature, and bonds to most materials including glass and glass fabrics, ceramics, wood, leather, most metals, and many plastics. AA-BOND 2110 is strong, tough, resilient, has superior mechanical impact and thermal shock resistance characteristics, and is also highly resistant to weather, water, gases and vapors, most petroleum products and fuels, salts, mild acids and alkalis, and many other organic and inorganic compounds.Appearance: Hazy off whiteCure Type: Heat cure or Room TemperatureBenefits:High impact strengthGood wettingLong pot life Mix Ratio by weight: 100:30/Resin:HardenerSubstrates: Staking components, bonding, laminating, repair applications, metals, glass, ceramics, wood and many plasticsTypical Application: PCB components, aerospace, anything where superior properties are requiredInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
mixed, uncured
Viscosity 60000 cP
60000 cP
Uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Adhesive Bond Strength 21.4 MPa
3100 psi
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 30.5 µm/m-°C
16.9 µin/in-°F
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 280 ohm-cm

@Temperature 80.0 °C
280 ohm-cm

@Temperature 176 °F
Dielectric Constant 4.7

@Frequency 1000 Hz
4.7

@Frequency 1000 Hz
Dielectric Strength 16.9 kV/mm
430 kV/in
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
0.31

@Frequency 1000 Hz
0.31

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 480 min
8.00 hour
4 hrs @ 25°C + 4 hrs @ 65°C
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Pot Life 60.0 min
60.0 min
100 grams, uncured
Descriptive Properties Value Comments
Thixotropic Index 6.6