ATI Wah Chang Spectrographic Grade Zirconium Oxide, ZrO2

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer ATI Wah Chang
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Wah Chang Spectrographic Grade Zirconium Oxide, ZrO2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Spectrographic Grade. A fine, white powder.Information provided by ATI Wah Chang
Physical Properties Metric English Comments
Particle Size 7.0 µm
7.0 µm
Particle Mesh Size 325 Mesh
325 Mesh
0.9
Specific Surface Area 2.0 m²/g
2.0 m²/g
B.E.T.
Molecular Weight 123.22 g/mol
123.22 g/mol
Component Elements Properties Metric English Comments
Boron, B 0.30 %
0.30 %
Sulfate, SO4 0.070 %
0.070 %