Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials NX10 Boron Nitride (BN) Powder

Category Ceramic , Nitride , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials NX10 Boron Nitride (BN) Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades are all fine hexagonal crystalline powders (95%-100% -325 mesh), and are available in a range of purities and surface areas to suit specific applications.NX10 has a mean particle size of approximately 10 microns and is a higher purity grade than NX9.Applications: GE Advanced Ceramics NX grades are candidates for use in a wide range of demanding applications for which BN is generally considered, including:Lubricants and release agents for high-temperature metal & glass processingRefractory coatingsBase material for hot pressed solids and metal-matrix or ceramic-metal compositesProcessing and final-product enhancement of plastics, including nucleation of solid and foamed products.Thermal management materials (adhesives, gap-fillers, encapsulants, polymer matrices, etc.) for electronics applicationsInformation provided by Momentive Performance Materials, formerly GE Advanced Ceramics.
Physical Properties Metric English Comments
Bulk Density 0.400 g/cc
0.0145 lb/in³
Tap Density
Particle Size 0.20 - 0.50 µm
0.20 - 0.50 µm
Crystal Size
10 µm
10 µm
Mean
Specific Surface Area 14 m²/g
14 m²/g
Descriptive Properties Value Comments
Calcium Max 0.01 %
Carbon 0.1%
Color White
Crystal Type Hexagonal (Graphitic)
Oxygen 0.9-1.2%
Sol. Borate 0.1%