Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 280 ohm-cm @Temperature 80.0 °C |
280 ohm-cm @Temperature 176 °F |
|
Tra-Con Tra-Bond 2110 High Impact Epoxy Staking Compound TRA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Volume Resistivity | 280 ohm-cm @Temperature 80.0 °C |
280 ohm-cm @Temperature 176 °F |
|
Atom Adhesives AA-BOND 2110 Epoxy Adhesive AA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, no.. |