Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 21.4 MPa | 3100 psi | Stainless-Stainless; Tensile Lap Shear |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Adhesive Bond Strength | 21.4 MPa | 3100 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond F194 Anaerobic Adhesive System TRA-BOND F194 is a high strength, anaerobic adhesive system designed for use in fiberoptic terminations or any applications requiring bond lines below .005". This system bonds well to all types of g.. |
|||
Adhesive Bond Strength | 21.4 MPa | 3100 psi | |
Trelleborg Emerson & Cuming Eccobond® 45 Two-Component General Purpose Epoxy Adhesive Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of .. |
|||
Adhesive Bond Strength | 21.4 MPa | 3100 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 2110 High Impact Epoxy Staking Compound TRA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Adhesive Bond Strength | 21.4 MPa | 3100 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
Tra-Con Tra-Bond 216E01 Non-Sag Dam Applications Adhesive TRA-BOND 216E01 is a thixotropic, two-part adhesive formulated specifically for applications where a high-fill, non-sag adhesive is required. TRA-BOND 216E01 works in concert with TRA-BOND 216E02 to.. |
|||
Adhesive Bond Strength | 21.4 MPa @Temperature 25.0 °C |
3100 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-2/E Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Adhesive Bond Strength | 21.4 MPa | 3100 psi | |
Atom Adhesives AA-BOND 2110 Epoxy Adhesive AA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, no.. |