Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | Recommended |
Nye Lubricants UniFlor 8710 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Parker Chomerics THERM-A-FORM 1641 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Parker Chomerics THERM-A-FORM 1642 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Parker Chomerics SOFT-SHIELD® 3500 Plated-Fabric Wrapped Foam Economical EMI Shielding Gasket for Electronics Description: The SOFT-SHIELD® 3500 fabric cover foam [FOF] product family is a group of low-closure force EMI/EMC gaskets. SS3500 offers a low cost/ low closure force competitive solution for EMI s.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Freudenberg Simrit SC1210 S310 Silicone Elastomer Excellent material for static service at extreme (hot or cold) temperatures. Outstanding flex and fatigue life. Very good for ozone and UV radiation service as well as for resistance to fungal and b.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Zotefoams Plastazote® LD15FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Zotefoams Plastazote® LD24FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Zotefoams Plastazote® LD24LC Low Density Polyethylene Foam, Large Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Tra-Con Tra-Bond FDA23 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-23 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admini.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Tra-Con Tra-Cast F311 Optically Transparent Semi-Flexible Casting System TRA-CAST F311 is a clear, low viscosity epoxy formulation developed for molding, embedding, casting and potting applications where clarity, toughness, long pot-life and superior impact properties ar.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Trelleborg S565 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Trelleborg S850 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Tra-Con Tra-Bond 2110 High Impact Epoxy Staking Compound TRA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Tra-Con Tra-Bond 2156 Heat Conductive Electrically Insulating Compound TRA-BOND 2156 is a thixotropic (smooth paste) thermally conductive epoxy system. It is used for staking heat sinks, transistors, diodes, resistor, integrated circuits and other heat-sensitive compon.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Tra-Con Tra-Bond 2158 Heat Conductive Electrically Insulating Compound TRA-BOND 2158 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Dow Corning MOLYKOTE® 33 EXTREME LOW TEMPERATURE BEARING GREASE, MEDIUM Phenyl-methyl silicone grease for extreme low temperaturesInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | ASTM D 3575 |
Eurofoam Polycell PLZ 45 Polyethylene Foam Information provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | ASTM D 3575 |
Eurofoam Siliconcell 412/BT 130 Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Atom Adhesives AA-BOND FDA16 Epoxy Adhesive AA-BOND FDA16 is a medium viscosity epoxy resin system specifically developed for medical device applications. AA-BOND FDA16 has been tested in accordance with USP biological reactivity tests, in vi.. |
|||
Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | |
Zotefoams Plastazote® LD15 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |