Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6906 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6907 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6007 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6009 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6010 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6013 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6201 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6202 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6205 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6403 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6605 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6001 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6204 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6207 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6701 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6803 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6804 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6808 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6811 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | |
Lord Adhesives 304 General Purpose, High Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 480 min | 8.00 hour | |
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 480 min | 8.00 hour | 4 hrs @ 25°C + 4 hrs @ 65°C |
Tra-Con Tra-Bond 2126 Black Opaque Epoxy Adhesive TRA-BOND 2126 is recommended for those modern photographic, industrial, and laboratory bonding and laminating applications where an easy-to-use, black (opaque) epoxy adhesive system with high perfor.. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Cure Time | 480 - 600 min | 8.00 - 10.0 hour | |
3M AC-370 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® RC8009 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® TL5042 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Average value: 880 min Grade Count:3 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Cure Time | 480 - 720 min | 8.00 - 12.0 hour | Time to Handling Strength |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6903 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |