Material Notes:
AA-BOND 2101 is a clear medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and electrical performance properties are required. AA-BOND 2101 easily mixes and cures at room temperature, and develops strong, durable, tough bonds to most clean, dry material surfaces. The fully cured AA-BOND 2101 bonds are great electrical insulators which also provide excellent resistance to weather, galvanic action, many mild acids and alkalis, salt solution, petroleum solvents, lubricating oil, gasoline, jet fuels, alcohol, and many other organic and inorganic materials.Appearance: Slight haze/ClearCure Type: Heat cure or Room TemperatureBenefits:Resistant to many organic/inorganicStrong bond strengthDurable Mix Ratio by weight: 100:25/Resin:HardenerSubstrates: Metals, ceramics, glass, glass fabrics, wood leather and rigid plastics Typical Application: Laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and electrical performance properties are required.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
mixed, uncured
Solids Content 100 %
100 %
uncured
Viscosity 17500 - 19500 cP
17500 - 19500 cP
Uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
Adhesive Bond Strength 20.7 MPa
3000 psi
Alum to Alum
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 62.0 °C
144 °F
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+15 ohm-cm
6.00e+15 ohm-cm
5.00e+9 ohm-cm

@Temperature 100 °C
5.00e+9 ohm-cm

@Temperature 212 °F
Dielectric Constant 4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Dielectric Strength 14.6 kV/mm
370 kV/in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30.0 min
30.0 min
uncured
Shelf Life 12.0 Month
12.0 Month
uncured