Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel lap shear |
Resinlab® CYNERGY CA6601 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 854-1 Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Bond F112 Fiber Optic Epoxy Adhesive TRA-BOND F112 is a long pot life, impact resistant, fiber-optic adhesive. This two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. This .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond F114BK01 Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114BK01 is a low viscosity, room temperature cure, epoxy system that contains no solvents, has excellent wicking and wetting characteristics, and adheres strongly to glass, ceramics, most .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive TRA-BOND F202 is a clear, low viscosity epoxy adhesive recommended for photonic applications requiring exposure to high temperatures or chemical and environmental resistance. This 100% solids system.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Varies with substrates |
Loctite® 312 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, cured 8 hrs |
Tra-Con Tra-Bond 2202 Low Viscosity/High Temperature Epoxy Adhesive TRA-BOND 2202 is a low viscosity, high temperature cure epoxy resin system developed for rigid laminating, filament winding, potting and bonding applications where a clear, almost transparent adhesi.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | |
Trelleborg Emerson & Cuming Eccobond® 2780-45 One-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming 2780-45 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveFilled, pourable, high temperature resistant, epoxy adhesive. Long term resistance to boiling glycol. Exc.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | |
Trelleborg Emerson & Cuming Eccobond® A 359 One-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming A 359 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveAluminum filled, heat curing, epoxy adhesive. Sag resistant. Exceptional thermal and chemical resistance. H.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Grit blasted steel |
Loctite® 426 Toughened Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel/Steel; Varies with substrates |
Loctite® 609 General Purpose Retaining Compound Retainers: Loctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel/Steel; Varies with substrates |
Loctite® 675 Medium Strength Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Adhesive Bond Strength | 20.7 - 41.4 MPa | 3000 - 6000 psi | Varies with substrates |
Loctite® Durabond® E-214HP Epoxy Adhesive Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific.. |
|||
Adhesive Bond Strength | >= 20.7 MPa | >= 3000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-106 Unfilled Epoxy Adhesive A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc. |
|||
Adhesive Bond Strength | >= 20.7 MPa | >= 3000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-130M-1 Unfilled Epoxy Adhesive A two-component, non-hazmat, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc. |
|||
Adhesive Bond Strength | >= 20.7 MPa | >= 3000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-135 Unfilled Epoxy Adhesive A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-135 has excellent bond strength to various substrat.. |
|||
Adhesive Bond Strength | 20.7 MPa @Temperature -54.4 °C |
3000 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-7/W Epoxy Adhesive, 3:2 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 931-1T1N1 Thixotropic Epoxy Encapsulant TRA-BOND 931-1T1N1 epoxy encapsulant is designed for good adhesion, providing strong resilient bonds to a wide variety of substances. This is a thixotropic version of TRA-BOND 931-1.Information prov.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 2 hrs @ 70°C |
Tra-Con Tra-Bond 970-1N1 General Purpose Epoxy Adhesive TRA-BOND 970-1N1 is a general purpose epoxy that exhibits sag resistance and excellent bond strength to a wide variety of substrates. Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114 is a clear, low viscosity, room temperature cure, epoxy system with good optical properties that contains no solvents, has excellent wicking and wetting characteristics, and adheres st.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Adhesive Bond Strength | 20.7 - 34.5 MPa | 3000 - 5000 psi | Varies with substrates |
Loctite® Durabond® E-20HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Alum to Alum |
Atom Adhesives AA-BOND 2101 Epoxy Adhesive AA-BOND 2101 is a clear medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and el.. |
|||
Adhesive Bond Strength | 20.7 - 34.5 MPa | 3000 - 5000 psi | Varies with substrates |
Loctite® Durabond® E-60HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |