Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 152 MPa
22000 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Strength 231 MPa
33500 psi
ASTM D790
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.61 J/cm
18.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
425 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
ASTM D648