Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 32.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E831 |
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E831 |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E831 |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N2033THL Nylon 6 (DAM) Information provided by Ravago. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature -40.0 - 149 °C |
18.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Semitron® ESd 410C- CM Dissipative Polyetherimide(ASTM Product Data Sheet) |
|||
CTE, linear | 32.4 - 50.4 µm/m-°C | 18.0 - 28.0 µin/in-°F | Average value: 39.0 µm/m-°C Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
CTE, linear | 32.4 - 117 µm/m-°C | 18.0 - 65.0 µin/in-°F | Average value: 70.3 µm/m-°C Grade Count:71 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear | 32.4 - 68.0 µm/m-°C | 18.0 - 37.8 µin/in-°F | Average value: 53.8 µm/m-°C Grade Count:11 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
CTE, linear | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Ensinger Sintimid™ V 15% graphite Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® NL-30GF/000 FR Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Electrafil® J-50/CF/10 Polycarbonate, 10% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Millennium III Glass Filled PC Structural Sheet Description: Structural SheetInformation provided by Spartech. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
CTE, linear | 32.4 µm/m-°C | 18.0 µin/in-°F | |
TriStar TriSteel AT Metal Backed PTFE Bearing System Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li.. |
|||
CTE, linear | 32.4 µm/m-°C | 18.0 µin/in-°F | |
Trelleborg Emerson & Cuming EP679 Patch Paste Blue patch pasteAll information provided by Trelleborg Emerson & Cuming |
|||
CTE, linear | 32.4 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D-3386 |
CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board REN SHAPE 5008 is a tooling board specifically designed for use in vacuum forming. It is designed for use up to 250°F and is well suited for building vacuum forming molds as well as master models,.. |
|||
CTE, linear | 32.4 µm/m-°C | 18.0 µin/in-°F | |
CMT Materials HYTAC® WF High Strength High Clarity 450°F Epoxy Syntactic HYTAC-WF is an excellent high temperature epoxy syntactic material that provides improved clarity when forming APET and other clear polymers plus reduces sticking of difficult to process polymers su.. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermylene® P-40FG-0860 40% Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermylene® P6-40FG-0100 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 2150 High Performance Epoxide Ceramic-Filled, Fast-Setting, High Vibration Resistance and Bond Strength. Ideal for bonding ceramic wear tiles. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 2220 High Performance Epoxide Ceramic-Filled, High Chemical Resistance, Machinable. For Repairing Deeply-Corroded Parts. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 526N High Performance Epoxide Clear-Amber, 1:1 System for Tough Bonding Applications Also available filled with aluminum oxide (Alumina) or pigments |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermylene® P6-40FB-Y947 40% Glass Fiber/Glass Bead, Heat Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermylene® P6-40FG-0684 40% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 32.4 - 109 µm/m-°C | 18.0 - 60.6 µin/in-°F | Average value: 76.5 µm/m-°C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
CTE, linear | 32.4 µm/m-°C @Temperature 20.0 °C |
18.0 µin/in-°F @Temperature 68.0 °F |
ASTM D1525 |
PlastxWorld CEVIAN® S5230 30% GF PC/ABS alloy Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld .. |