Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 152 MPa | 22000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ CTX-502 Natural Polyether Imide (PEI) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | |
Pacific Sintered Materials SS-316-RH 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced Information provided by Ravago. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | 0.125 in; ASTM D638 |
Matrixx Group 85S7451 Flame Retardant 45% Glass Reinforced PET
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |
|||
Tensile Strength, Yield | 152 - 230 MPa | 22000 - 33400 psi | Average value: 183 MPa Grade Count:6 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Yield | 152 MPa @Thickness 3.20 mm |
22000 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID HI2302A(W) PA6+GF30%, High Impact Feature: Injection Molding, PA6+GF30%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | .01% permanent set |
Meehanite GA-50 Flake Graphite Cast Iron Type GA-50 combines high strength, toughness, wear resistance and damping capacity with excellent machinability. Responds well to heat treatment, local and surface hardening.General Meehanite infor.. |
|||
Tensile Strength, Yield | 152 MPa @Thickness 3.20 mm |
22000 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 152 MPa @Strain 0.200 %, Temperature 871 °C |
22000 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF33 IM L NAT001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedAppearance.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 C10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightFeatures: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF20 L BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES HiFill® PBT GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES HiFill® PES GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 IM1 HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant, Halogen Free and Impact ModifiedAppearance: BlackI.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedAppearance: BlackInformation.. |
|||
Tensile Strength, Yield | 152 - 359 MPa | 22000 - 52000 psi | 0.2% offset |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Ashley Polymers Ashlene® 525LD-33G Nylon 66, 33% Glass Reinforced High impact Nylon 66 reinforced with 33% glass fibers, lubricated.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Cheng Yu Plastic A708G3 SAN, 30% Glass Fiber |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylex® P1310G40 HB Polycarbonate, 40% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Tensile Strength, Yield | 152 MPa | 22000 psi | ASTM D638 |
Ashley Polymers Ashlene® PE126 PET Polyester, 30% Glass Reinforced PET Polyester, with 30% glass reinforcement.Data provided by the manufacturer |