Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.61 J/cm @Temperature 23.0 °C |
18.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Valox® 414 PBT (Asia Pacific) 40% GR, increased strength/stiffness vs unreinforced. Non-flame retardant. For appliance handles, spotlights, electric motors, pump housings etc.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Izod Impact, Unnotched | 9.61 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF30 HR HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and Hydrolysis ResistantFeatures: Heat Stabilized and Hydrolys.. |
|||
Izod Impact, Unnotched | 9.61 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 HR HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Hydrolysis Resistant Appearance: .. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® RMT-10 10% Talc-Reinforced Polypropylene, High Impact Polifil® RMT series compounds are high impact polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and high heat deflection resis.. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 9.61 - 12.3 J/cm | 18.0 - 23.0 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |