Polymer Property : Flexural Modulus = 8.48 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Nylene® 9543 , 43% Glass Reinforced Nylon 6/12
Description: Nylene® 9543 s a 43% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour..
Flexural Modulus 8.48 GPa

@Temperature 22.8 °C
1230 ksi

@Temperature 73.0 °F
ASTM D790
Celanese Celanex® 3309HR PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass reinforced, hyd..
Flexural Modulus 8.48 GPa

@Temperature 22.8 °C
1230 ksi

@Temperature 73.0 °F
ASTM D790
Celanese Celanex® 3309HRLM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass filled PBT, h..
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
LNP Lubricomp® EFL-4544 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Flexural Modulus 8.48 GPa
1230 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF0069P PC
LNP THERMOCOMP* DF0069P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant.
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific)
LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber.
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10
LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11
LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber.
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Entec Hylox® 9230BK PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Celanese CELANEX 3309HR PBT, 30% Glass Reinforced
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.Information provided by C..
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Celanese CELANEX 3309HRLM PBT, 30% Glass Reinforced
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability. lIt is a asermarkable ..
Flexural Modulus 8.48 GPa

@Temperature 22.8 °C
1230 ksi

@Temperature 73.0 °F
ASTM D790
Celanese Celanex® 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityTo avoid hydrolytic degradation during processi..
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
RTP Company RTP 205D  Nylon 6/12 (PA 6/12) Glass Fiber 30%  (discontinued **)
Glass Fiber 30%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Flexural Modulus 8.48 GPa
1230 ksi
ASTM D790
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant  (disconti