Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E831
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified
Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
CTE, linear 32.4 µm/m-°C

@Temperature -20.0 - 150 °C
18.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E831
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
CTE, linear 32.4 µm/m-°C

@Temperature -20.0 - 150 °C
18.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E831
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced
Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N2033THL Nylon 6 (DAM)
Information provided by Ravago.
CTE, linear 32.4 µm/m-°C

@Temperature -40.0 - 149 °C
18.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Semitron® ESd 410C- CM Dissipative Polyetherimide(ASTM Product Data Sheet)
CTE, linear 32.4 - 50.4 µm/m-°C
18.0 - 28.0 µin/in-°F
Average value: 39.0 µm/m-°C Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
CTE, linear 32.4 - 117 µm/m-°C
18.0 - 65.0 µin/in-°F
Average value: 70.3 µm/m-°C Grade Count:71
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
CTE, linear 32.4 - 68.0 µm/m-°C
18.0 - 37.8 µin/in-°F
Average value: 53.8 µm/m-°C Grade Count:11
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
CTE, linear 32.4 µm/m-°C
18.0 µin/in-°F
ASTM D696
Ensinger Sintimid™ V 15% graphite Polyimide (PI)  (discontinued **)
SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V..
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® NL-30GF/000 FR Nylon 6/12, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Electrafil® J-50/CF/10 Polycarbonate, 10% Carbon Fiber Reinforced
Carbon Fiber Reinforced
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Millennium III Glass Filled PC Structural Sheet
Description: Structural SheetInformation provided by Spartech.
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
CTE, linear 32.4 µm/m-°C
18.0 µin/in-°F
TriStar TriSteel AT Metal Backed PTFE Bearing System
Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li..
CTE, linear 32.4 µm/m-°C
18.0 µin/in-°F
Trelleborg Emerson & Cuming EP679 Patch Paste
Blue patch pasteAll information provided by Trelleborg Emerson & Cuming
CTE, linear 32.4 µm/m-°C

@Temperature -30.0 - 30.0 °C
18.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D-3386
CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board
REN SHAPE 5008 is a tooling board specifically designed for use in vacuum forming. It is designed for use up to 250°F and is well suited for building vacuum forming molds as well as master models,..
CTE, linear 32.4 µm/m-°C
18.0 µin/in-°F
CMT Materials HYTAC® WF High Strength High Clarity 450°F Epoxy Syntactic
HYTAC-WF is an excellent high temperature epoxy syntactic material that provides improved clarity when forming APET and other clear polymers plus reduces sticking of difficult to process polymers su..
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P-40FG-0860 40% Glass Fiber Reinforced
Information provided by Asahi Thermofil
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P6-40FG-0100 40% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
Aremco Aremco-Bond™ 2150 High Performance Epoxide
Ceramic-Filled, Fast-Setting, High Vibration Resistance and Bond Strength. Ideal for bonding ceramic wear tiles.
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
Aremco Aremco-Bond™ 2220 High Performance Epoxide
Ceramic-Filled, High Chemical Resistance, Machinable. For Repairing Deeply-Corroded Parts.
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
Aremco Aremco-Bond™ 526N High Performance Epoxide
Clear-Amber, 1:1 System for Tough Bonding Applications Also available filled with aluminum oxide (Alumina) or pigments
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P6-40FB-Y947 40% Glass Fiber/Glass Bead, Heat Stabilized
Information provided by Asahi Thermofil
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P6-40FG-0684 40% Glass Fiber Reinforced, Heat and UV Stabilized
Information provided by Asahi Thermofil
CTE, linear 32.4 - 109 µm/m-°C
18.0 - 60.6 µin/in-°F
Average value: 76.5 µm/m-°C Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D1525
PlastxWorld CEVIAN® S5230 30% GF PC/ABS alloy
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld ..