Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name Corr-Paint™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low viscosity, green coating for power resistors to 1100°F (593°C)
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
Solids Content 39.5 %
39.5 %
by volume
48.5 %
48.5 %
by weight
Volatile Organic Compounds (VOC) Content 117 g/l
117 g/l
Viscosity 500 - 750 cP
500 - 750 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
64.3 microns
2.53 mil
estimated wet film thickness
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 593 °C
1100 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 48.9 °C
50.0 - 120 °F
Application Temperature
Dry Time 1 hour
1 hour
Handling
2 hour
2 hour
Touch
>= 2.5 hour
>= 2.5 hour
Recoat
Cure Time >= 60.0 min
>= 1.00 hour
Air Set prior to curing
45.0 min

@Temperature 232 °C
0.750 hour

@Temperature 450 °F
Adequate ventilation is required when curing these products. Outgassing will occur above 300°F and cease after 750°F. An additional 30 minutes is required at the highest service temperature if service temperature is below 750°F.
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Green
Dry Film Coverage ft2/gal 634
at 1 mil
Thinner Butyl Cellosolve/Water