Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 10.0 - 177 °C | 50.0 - 350 °F | Average value: 73.0 °C Grade Count:3 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 529 High Temperature Specialty Coatings Silicone Transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 529VHV High Temperature Specialty Coatings Silicone Very high viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-BN (SC) High Temperature Refractory Coating This highly-filled boron nitride solution is extremely lubricious and inert. It is non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN(SC) .. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass Glass coating for producing hermetic seals in porous ceramics and refractories to 1450 ºF. Used for sealing high vacuum components, resistance temperature devices, and other electrical sensors. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-GLT High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, light-green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps,.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C). |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f.. |